All-Alci
All-Alci

Joint Filler

DEFINITION

Cement-based, fiber and polymer reinforced, high-performance thermal insulation board plaster.

AREAS OF USE
  • As plaster on polystyrene boards (XPS; Extruded Polystyrene or EPS; Expanded Polystyrene),
  • For repair purposes; at the joints of main structural elements.
  • Stone wool
  • For corner and parapet cracks.
  • For plastering purposes (up to 5 mm).
  • On aerated concrete surfaces.
  • As a thin plaster over rough plaster.
FEATURES / ADVANTAGES
  • Provides high adhesion to thermal insulation boards.
  • Allows the system to breathe due to its vapor permeability.
  • Provides easy and long-term working conditions.
  • Provides a smooth and aesthetic appearance on interior and exterior surfaces.
  • Absorbs small stresses.
  • Minimizes crack formation with fiber and polymer reinforcement.
PRODUCT INFORMATION
  • Form: Cement-based, fiber and polymer-reinforced powder
  • Color: Gray
  • Packaging: 25 kg kraft bag
  • Shelf Life: 12 months in a dry environment without moisture
  • Unit Weight: 1300 ±100 g/lt
  • Usable Time of the Mortar: 2 - 2.5 hours
  • Working Time: 25 min
  • Application Thickness: 3 - 5 mm
SURFACE PREPARATION

The panel to be applied must be properly adhered to the substrate.

Gaps between panels must be filled appropriately, and the surface must be smooth.

APPLICATION

Pour 6-7 liters of water into a clean container large enough to hold one bag. Slowly add Allkim Flex Thermal Insulation Panel Mortar to the water and mix with a low-speed mixer until a homogeneous mixture is obtained. After the mixed mortar has rested for 5 minutes, it is mixed again for 1-2 minutes and made ready for use. The prepared mortar is applied to the thermal insulation boards with a thickness of 2 mm, and plaster mesh is laid to ensure adhesion to the surface. To prevent cracking, the reinforcement mesh should be applied overlapping by 10 cm at the joints. Then, a second coat of fine plaster is applied with a thickness of 2 mm. The material, which has started to harden, is smoothed and troweled.

APPLICATION TOOLS

Hand mixer, steel trowel, spatula, rubber trowel

SHELF LIFE

1 year from the date of manufacture in dry and moisture-free conditions.

CONSUMPTION

Depending on the surface to be applied and the thickness, 4-5 kg/m² for a thickness of 3-4 mm.

WARNINGS AND PRECAUTIONS
  • The application temperature should be between +5 ⁰C and +35 ⁰C.
  • Avoid application in very humid and very hot weather.
  • Do not apply on surfaces at risk of freezing.
  • After plaster application, the surface should be moistened at regular intervals.
  • Coating, painting, and similar applications should begin 7 days after plaster application.
  • Avoid constant contact of the material with eyes and skin; do not inhale dust from the material.
  • All tools used should be cleaned with water before they dry.
  • The information provided is valid for application areas with a temperature of 23 ± 2 ⁰C and humidity of 50 ± 5%.
PRODUCT DEFINITION

Cement-based, high-performance, water-repellent, single-component joint filler containing polymer additives.

APPLICATION AREA

Used for filling 0-6 mm joints in indoor and outdoor areas, on walls and floors, and on floors with heavy foot and load traffic.

Please consult us for all other applications.

APPLICATION LIMIT

Not suitable for use in areas exposed to high pressure (> 100 bar) and chemicals, or in areas requiring hygiene.

Not suitable for swimming pools.

Not suitable for floors prone to deformation, such as underfloor heating systems.

REFERENCE STANDARDS

TS EN 13888 CG1

QUALITY CERTIFICATES

CE

These values were obtained from tests conducted under laboratory conditions at 23±2 °C and 50% relative humidity, and reflect performance after 28 days. Values may vary due to differences in the construction site environment.

WARNINGS AND RECOMMENDATIONS

No foreign materials should be added under any circumstances. After application, all tools used should be washed with water before they dry. Mortar that has passed its use-by date should not be reused by adding water. For high performance, the application area should be moistened with water the next day. To avoid yellowing in white and light-colored grout, ceramic tiles should not be soaked in water.

SURFACE PREPARATION

The surface must be clean, smooth, and solid.

The ambient temperature should be between +5 °C and +30 °C.

Grout joints must be cleaned and walls moistened before application.

APPLICATION CONDITIONS

The ambient temperature should be between +5 °C and +35 °C.

Application should not be carried out in very humid, very hot, or excessively windy weather.

It should not be applied on frozen, thawing, or surfaces at risk of freezing within 24 hours.

APPLICATION INSTRUCTIONS

Slowly pour 20 kg of Allkim Flex Joint Filler into 7.5-8 liters of water and mix with a low-speed mixer until homogeneous.

Allow the prepared mortar to rest for 5-10 minutes, then mix again before application.

The mortar should be filled into the joints with a rubber trowel and any excess should be scraped off.

After 15-30 minutes, the surface should be cleaned with a damp sponge.

CONSUMPTION

Varies depending on the application.

PACKAGING

20 kg bag (60 pieces per pallet, 1200 kg)

PALLET DIMENSIONS

80x110 cm

COLOR

White, gray, beige, and other colors

APPLICATION TOOLS

Hand mixer, trowel, rubber-tipped trowel, sponge-tipped trowel, squeegee, sponge, brush

SHELF LIFE

1 year from the date of manufacture in a dry, moisture-free environment

Technical Specifications

PERFORMANCE INFORMATION

Usable Time Max 1 hour
Full Hardening Time 24 hours
Time to Open to Traffic 24-48 hours
Flexural Strength ≥ 2.5 N/mm² (TS EN 12808-3)
Flexural Strength After Freeze-Thaw Cycle ≥ 2.5 N/mm²
Compressive Strength ≥ 15 N/mm²
Compressive Strength After Freeze-Thaw Cycle ≥ 15 N/mm²
Abrasion Resistance ≤ 2000 mm³ (TS EN 12808-2)
Shrinkage ≤ 3 mm/m (TS EN 12808-4)
Water Absorption 30 min. / 4 hours ≤ 5 g / ≤ 10 g (TS EN 12808-5)
Fire Reaction Class A1 (TS EN 13501-1)